Test | Status | Code Input and Output |
---|---|---|
1 | Pass |
filetext = fileread('count_pits.m')
assert(isempty(strfind(filetext, 'rand')))
assert(isempty(strfind(filetext, 'fileread')))
assert(isempty(strfind(filetext, 'assert')))
filetext =
'function ans = count_pits(x)
[r,c] = find(x);
sum(max(conncomp(graph(max(abs(r-r'),abs(c-c'))<=1))))
end
%This code written by profile_id 734801
'
|
2 | Pass |
x = 1;
y_correct = 1;
assert(isequal(count_pits(x),y_correct))
ans =
1
|
3 | Pass |
x = 0;
y_correct = 0;
assert(isequal(count_pits(x),y_correct))
ans =
0
|
4 | Pass |
x = [1 0 1 0 1];
y_correct = 3;
assert(isequal(count_pits(x),y_correct))
ans =
3
|
5 | Pass |
x = [0 0 1 0 0 0 0 0 0 0
0 1 1 0 0 0 0 0 0 0
0 0 1 1 0 0 0 1 1 0
0 0 0 1 0 0 0 1 1 0
0 0 0 0 0 0 0 0 0 0
0 0 0 0 0 0 0 0 0 0
0 0 1 0 0 0 0 1 0 0
0 0 0 1 0 0 0 1 1 0
0 0 0 0 0 0 0 0 1 0
0 0 0 0 1 1 0 0 0 0];
assert(isequal(count_pits(x),5))
ans =
5
|
6 | Pass |
x = [ 0 0 0 1 0 0 0 0 0 0 0 0 0 0 1 0 0 0 1 0
0 0 0 0 0 0 0 0 0 1 1 0 1 0 1 0 0 0 0 0
0 1 1 0 0 0 0 0 0 0 1 0 0 1 1 0 0 0 0 0
0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 1 0 0 0 1
0 1 1 0 0 1 0 1 0 0 0 0 0 0 1 1 0 0 0 0
0 0 0 1 0 0 1 0 0 0 0 0 0 0 0 0 0 1 0 1
0 0 0 1 0 1 0 0 0 0 0 0 1 0 1 0 0 0 0 0
0 0 0 1 0 0 0 0 0 0 0 0 0 0 0 1 0 0 1 0
1 0 0 0 1 1 0 0 0 0 0 0 0 0 0 0 0 0 0 1
0 0 0 0 0 0 0 0 0 0 1 0 0 0 1 0 0 0 0 0
0 0 0 0 1 0 0 0 0 1 0 0 1 0 0 0 0 0 0 0
0 0 0 0 0 0 0 0 1 0 0 0 0 0 0 1 0 0 0 0
0 0 0 0 0 0 0 0 1 0 0 0 0 0 1 0 0 0 0 0
0 1 0 0 0 0 0 0 0 0 0 0 1 0 0 1 0 1 0 1
0 0 0 0 0 0 0 0 0 0 0 0 1 0 1 0 0 0 1 0
1 0 0 0 0 0 0 0 0 0 0 1 0 1 0 0 0 0 0 0
1 0 0 0 0 0 0 0 0 0 0 0 1 0 0 0 0 0 1 0
0 1 0 0 0 0 0 0 1 0 0 1 0 1 0 0 1 1 0 0
0 0 0 0 0 1 0 1 0 0 0 0 0 0 0 0 1 1 0 0
0 0 1 0 0 0 0 0 0 0 0 0 0 0 0 0 0 1 0 0];
assert(isequal(count_pits(x),26))
ans =
26
|
7 | Pass |
x = [0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 1 0 0 0
0 1 0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 1 0 0
1 0 1 0 0 0 0 0 0 1 0 0 0 0 0 0 0 0 0 0
0 0 0 0 0 0 0 0 1 0 0 1 0 0 0 0 0 0 0 0
0 0 0 0 0 0 0 0 0 0 0 0 0 1 0 0 1 1 1 0
1 0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 1 1 0 0
0 0 0 0 0 0 1 0 0 0 0 0 1 1 0 0 0 0 1 0
0 1 0 1 0 0 0 0 0 0 0 1 0 0 0 1 1 1 0 0
0 0 0 0 1 0 0 0 0 0 0 0 1 1 1 1 0 0 1 0
0 0 0 0 1 0 0 0 1 1 0 0 0 0 0 0 0 0 0 0
0 0 0 0 0 0 0 0 0 0 1 0 1 0 0 1 0 0 0 0
0 0 0 0 0 0 0 0 0 0 1 1 0 1 0 0 0 0 0 0
0 0 0 0 0 0 0 0 0 0 0 0 0 0 1 0 1 0 0 1
0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 1 0 0 0
0 0 0 1 0 0 0 0 0 1 0 0 0 1 1 0 0 0 0 1
1 0 0 0 0 0 0 0 1 0 0 1 0 0 0 0 0 0 0 0
0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 0
0 0 0 0 0 0 0 0 0 0 0 0 0 1 0 0 0 0 0 0
0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 1 0
0 1 0 0 0 1 0 0 0 0 0 0 0 0 0 1 0 0 1 0];
assert(isequal(count_pits(x),25))
ans =
25
|
8 | Pass |
x = [1 0 1 0 1 0 0 1
0 0 0 0 0 0 0 0
0 0 0 1 0 0 1 0
0 0 0 1 1 1 0 1
0 0 0 0 1 0 0 0];
assert(isequal(count_pits(x),5))
ans =
5
|
9 | Pass |
x = eye(20);
assert(isequal(count_pits(x),1))
ans =
1
|
10 | Pass |
x = [1 0 0 0 0 0 0 0 0 1
0 0 0 0 0 0 0 0 0 0
1 1 0 0 0 0 0 0 0 0
0 0 0 0 1 0 0 0 0 0
0 0 0 0 0 0 0 0 1 0
0 0 1 0 0 0 0 1 0 0
0 0 0 0 0 0 0 0 0 0
0 0 0 0 1 0 0 0 0 1
0 0 0 0 0 0 1 0 0 0
0 0 0 0 0 0 1 0 0 0];
assert(isequal(count_pits(x),9))
ans =
9
|
11 | Pass |
x = [0 0 0 1 0 0 0 0 0 1 0 1 1 0 0
0 0 0 1 0 0 0 0 0 1 1 1 0 0 1
0 1 0 0 0 1 0 0 1 0 1 0 0 0 0
0 1 0 0 0 1 0 0 1 0 0 0 0 0 0
1 0 0 0 0 0 0 0 1 0 0 0 0 0 0
0 0 0 0 0 0 1 0 0 0 0 1 0 0 1
1 0 0 0 0 0 0 0 0 1 0 0 0 1 1
0 1 0 0 0 1 0 0 0 0 0 1 0 0 0
0 1 0 0 0 1 1 0 0 1 0 0 0 0 0
0 0 0 0 0 0 0 0 1 0 0 0 0 1 0
0 0 0 0 0 0 0 0 0 0 0 0 1 0 1
0 1 0 0 0 0 0 0 0 0 1 1 0 0 0
0 0 0 0 0 0 1 0 0 0 0 0 0 0 0
0 1 0 0 0 0 0 0 0 0 0 0 0 0 0
0 0 1 0 0 0 0 0 0 0 0 0 1 0 1];
assert(isequal(count_pits(x),19))
ans =
19
|
12 | Pass |
x = [0 0 0 0 0 0 0 1 1 0 0 0 1 0 0 0 0 0 1 1
0 1 0 0 1 0 0 0 0 1 0 1 0 0 1 0 0 1 0 0
0 0 0 0 0 0 0 0 0 0 1 0 1 0 1 0 0 0 0 1
0 0 1 0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 0
1 0 0 0 1 0 0 0 0 0 1 0 0 0 0 1 1 0 1 1
0 0 0 0 1 0 0 0 0 0 0 1 0 0 0 1 0 0 0 0
0 0 0 1 0 0 0 0 1 1 0 0 0 0 0 1 1 0 0 0
0 0 0 0 0 0 0 0 1 0 0 0 0 0 0 0 1 0 1 1
0 1 0 0 0 1 0 0 1 0 0 0 0 0 0 0 0 1 0 0
0 1 1 0 1 0 0 1 0 1 0 1 0 1 0 0 0 0 0 1
1 0 0 1 0 0 0 0 0 0 1 1 0 1 1 0 0 0 0 0
1 1 0 0 0 0 0 0 0 0 0 1 0 0 0 0 0 0 0 1
1 0 0 1 0 0 1 0 0 1 0 0 0 0 1 0 0 0 0 0
0 0 0 0 1 0 1 0 0 0 1 0 0 0 0 0 0 0 0 0];
assert(isequal(count_pits(x),21))
ans =
21
|
13 | Pass |
x = repmat([0 1;1 0],5,7);
assert(isequal(count_pits(x),1))
ans =
1
|
14 | Pass |
x = repmat([0 1;0 0],5,7);
assert(isequal(count_pits(x),35))
ans =
35
|
15 | Pass |
x = [0 0 1 0 0 0 0 0 0 0 0 0 0 0 0 0 1
0 0 0 0 1 0 1 0 1 1 0 0 1 0 1 1 0
0 0 0 1 0 1 0 1 0 0 1 1 0 1 0 1 1
0 0 0 0 1 0 0 0 0 0 0 0 1 0 1 0 1
1 0 0 1 0 0 0 1 1 1 0 1 0 0 0 0 0
1 0 0 1 1 0 0 0 1 1 0 0 0 1 1 0 0
0 0 0 0 0 1 1 0 1 1 1 0 0 0 1 1 0
0 0 0 0 0 0 0 1 0 1 0 0 0 1 0 0 0
0 0 0 1 1 1 0 0 0 1 0 0 0 0 0 1 1
1 0 1 0 0 0 0 0 1 0 0 0 1 0 1 0 1
0 0 0 0 0 0 1 0 0 0 0 0 0 0 0 1 0
1 0 0 1 1 0 0 0 1 0 0 1 0 0 1 0 0
0 1 0 0 0 1 0 0 0 0 1 0 0 0 0 1 0
0 0 0 0 0 1 1 1 0 0 0 1 0 0 1 1 0
0 1 0 0 1 0 0 1 0 0 0 1 0 0 1 0 0
0 0 1 1 0 0 0 0 1 0 0 1 0 0 0 0 0
0 1 0 1 0 0 0 0 0 0 0 1 0 1 0 0 0
0 1 0 0 0 1 0 0 0 1 1 0 1 0 0 1 0];
assert(isequal(count_pits(x),15))
ans =
15
|
16 | Pass |
x = [0 0 1 1 1 0 1 0 0 1 0 0 0 0 0 0
0 0 1 0 1 0 1 1 0 0 0 0 0 0 1 0
0 1 0 1 1 1 1 0 1 0 0 0 1 0 0 0
0 1 0 0 0 0 0 0 0 0 1 0 0 1 0 0
0 0 0 0 0 0 0 0 0 0 0 1 0 0 0 1
0 1 0 1 0 0 1 0 0 1 0 0 0 0 0 0
0 1 0 1 1 1 0 0 1 1 0 0 0 0 1 0
0 0 0 0 0 0 1 1 1 1 0 0 0 0 1 1
0 1 0 1 0 0 1 0 0 1 0 1 1 1 0 0
0 0 0 1 0 0 0 0 0 1 0 0 0 0 1 1
0 0 0 0 0 0 0 1 0 1 0 0 1 0 0 0];
assert(isequal(count_pits(x),13))
ans =
13
|
17 | Pass |
x = zeros(5);
assert(isequal(count_pits(x),0))
ans =
0
|
18 | Pass |
x = [ 0 0 0 0 0 0 0 1 0 1 0 0 0 0 0 1 0 0 0 1
1 0 0 1 0 0 0 0 0 0 0 0 0 0 1 0 0 1 1 1
1 0 0 0 1 0 0 0 0 0 0 0 0 1 1 0 0 0 1 0
1 0 0 1 0 0 0 0 1 1 0 0 0 1 0 1 0 0 0 0
1 1 0 1 0 0 1 0 0 0 1 1 0 0 0 1 1 1 0 1
0 1 0 0 1 1 0 0 0 0 0 0 0 0 0 0 1 0 0 1
0 0 0 0 1 1 1 0 0 0 0 1 0 0 0 0 1 0 1 1
1 1 0 0 0 1 1 0 1 1 0 1 1 0 1 1 0 0 0 1
0 0 0 1 0 1 0 1 0 0 0 1 0 0 0 1 0 0 1 0
1 0 0 0 0 0 0 0 1 0 0 0 0 1 0 0 1 0 1 1
0 0 0 0 0 0 0 1 0 0 1 0 1 0 0 0 1 1 1 0
1 0 0 0 0 0 1 0 0 0 0 0 1 1 1 0 0 0 0 1
1 1 0 0 0 1 0 0 0 1 0 1 0 0 0 0 0 0 0 0
0 1 0 0 1 0 0 0 0 0 0 1 1 0 1 0 1 0 0 1
0 0 0 1 0 0 0 1 1 0 0 0 0 1 0 0 0 1 0 1
0 1 0 1 0 1 1 0 0 0 1 1 0 0 0 0 1 0 0 0
1 0 0 0 0 1 1 1 1 0 0 0 0 0 0 1 1 0 1 0
0 0 1 0 1 0 0 0 0 1 0 0 0 1 1 1 0 0 0 0
0 0 1 0 1 0 0 1 0 0 0 0 0 0 0 0 0 1 0 0
1 0 0 1 0 1 1 0 1 0 0 1 0 0 0 0 0 0 0 0];
assert(isequal(count_pits(x),24))
ans =
24
|
19 | Pass |
x = [0 1 0 1 1 1 0 0 0 1 0 0 1 0 0 1 1 0 0 1
0 0 0 1 1 1 0 1 1 1 0 0 0 0 1 1 1 0 0 0
0 1 0 1 1 0 0 1 1 1 0 1 1 0 1 1 1 0 0 0
1 1 1 0 1 1 1 0 1 1 0 0 1 0 1 1 0 1 1 0
1 0 0 0 1 1 1 0 0 1 1 1 1 1 1 1 1 1 0 0
1 0 1 1 1 0 0 0 0 1 1 1 1 1 1 0 0 1 0 1
1 1 0 1 1 1 0 1 0 1 1 0 0 0 0 1 1 0 1 0
0 1 0 1 1 0 1 0 0 0 1 0 0 0 1 0 1 0 0 1
1 0 1 1 1 0 0 0 1 1 0 1 0 1 1 1 1 1 0 0
0 0 0 1 1 0 0 0 1 0 1 1 1 1 0 0 0 0 1 0
0 0 1 1 0 1 1 1 1 0 1 0 0 0 0 0 1 1 1 1
1 0 1 1 1 1 1 1 1 1 1 0 1 1 0 0 1 1 0 1
1 0 1 0 0 1 0 1 0 0 0 0 0 1 0 0 0 1 1 1
0 1 1 1 1 1 0 0 1 1 1 1 1 1 0 1 0 0 1 0
1 0 1 0 0 1 0 0 0 0 0 0 1 1 0 1 1 1 0 0
1 0 0 1 0 1 1 1 1 1 0 1 0 0 0 0 0 0 1 1
0 0 0 0 1 1 1 0 1 0 0 0 1 0 0 1 0 1 1 0
0 1 1 1 1 0 1 1 1 0 1 0 0 1 0 1 1 0 1 1
0 0 0 0 1 1 0 0 0 1 1 0 1 0 1 1 1 0 1 1
1 1 1 0 0 0 1 0 0 0 0 1 0 0 1 0 1 1 1 0];
assert(isequal(count_pits(x),5))
ans =
5
|
20 | Pass |
x = [ 0 1 0 0 0 0 1 0 0 0 0 0 0 0 0 0 0 1 1 0
0 0 0 0 0 1 0 0 0 1 0 0 0 0 1 0 0 0 0 0
0 0 0 0 0 1 0 0 0 0 0 0 0 0 1 1 0 1 0 0
0 1 1 0 0 0 0 1 0 0 0 0 0 0 0 0 0 0 0 0
0 0 0 0 0 0 0 0 1 1 0 0 0 0 0 0 0 0 0 0
0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 1
0 0 0 0 1 0 0 0 0 0 0 0 0 0 0 0 0 0 0 0
0 0 0 0 0 0 0 0 0 0 0 1 0 0 0 0 0 0 1 0
1 0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 1 0 1 0
0 0 1 0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 1
0 0 0 0 1 0 0 0 0 0 1 0 0 1 1 0 0 0 0 0
0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 1
0 0 0 0 0 0 1 0 0 0 1 0 0 1 0 1 0 0 0 0
0 0 0 0 0 0 0 0 0 0 0 0 1 0 0 0 1 0 0 0
0 0 0 0 0 0 0 1 0 0 0 0 0 1 1 0 0 0 0 0
0 0 0 0 0 0 1 1 0 0 0 0 0 0 0 0 0 0 0 0
0 1 0 0 0 0 0 0 0 0 0 1 0 0 0 0 0 0 1 0
0 0 0 0 1 0 0 0 0 0 0 0 0 0 0 0 0 0 0 0
0 0 0 0 0 0 0 1 1 0 0 0 0 0 0 0 0 0 1 0
0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 0 0];
assert(isequal(count_pits(x),30))
ans =
30
|
Sum all integers from 1 to 2^n
8418 Solvers
Getting the indices from a matrice
360 Solvers
123 Solvers
188 Solvers
429 Solvers
Find the treasures in MATLAB Central and discover how the community can help you!
Start Hunting!